TCS Line Primer
Surface Preparation: Pavement surface must be cleaned entirely of dust, dirt and debris.
Mixing Procedures: DO NOT DILUTE. STIR OR SHAKE THOROUGHLY BEFORE USING.
Application: TCS Line Primer can be rolled or brushed. Allow TCS Line Primer to dry completely before applying TCS Textured White Line Paint.
Important: Temperatures must be a minimum of 50ºF and rising both during application and for a period of at least 24 hours after application. Do not apply when rain is imminent in the forecast. Keep from freezing. Close container when not in use.
Coverage: 500 to 600 linear feet of 2-inch line per gallon.
Drying Time: TCS Line Primer should dry in 30 to 60 minutes under optimum drying conditions.
Clean Up: Wash tools in water before material dries.
VOC: This material contains less than 150 grams of volatile organic
compounds per liter.
Caution: KEEP FROM FREEZING. KEEP OUT OF REACH OF HILDREN. Do not take internally. If swallowed, call a physician immediately. In case of contact with eyes, flush immediately with water for 15 minutes and call a physician. Do not apply when rain is imminent. When not in use, keep container tightly closed and upright to prevent leakage. Do not store in direct sunlight or above 100 ºF. In case of spillage, absorb and dispose of in accordance with Federal, State and Local regulations.
Warranty: The statements made on this label are believed to be true and accurate and are intended to provide a guide for approved application practices. As workmanship, weather, construction, equipment utilized and other variables affecting results are all beyond our control. Tennis Court Supply warrants only that the material conforms to product specifications and any liability to the buyer or use of this product is limited to the replacement value of the product only. In no event shall tennis court supply be liable for any injury, loss or damage, either direct or incidental, special or consequential, however arising in connection with material or equipment furnished or work performed. Tennis Court Supply shall not, in any manner, be liable for any defects, variations or change in condition in the substructure over which its products are installed.